Polymer Property : Volume Resistivity = 1.0 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 0.010 - 1.0 ohm-cm
0.010 - 1.0 ohm-cm
IEC 60093
Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin
CF 30% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..