Electrical Properties Metric English Comments
Volume Resistivity 1.10e+13 ohm-cm
1.10e+13 ohm-cm
60°C for 1,000 hrs with 90% RH; JIS-K-6249
Fujipoly Industries Sarcon® GR-Fd Gap Filler Pad
Sarcon GR-d is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary. GR-Fd has a mesh embedded overall.Information provided b..
Volume Resistivity 1.10e+13 ohm-cm
1.10e+13 ohm-cm
70°C for 1,000 hrs; JIS-K-6249
Fujipoly Industries Sarcon® GR-m Gap Filler Pad
Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Volume Resistivity 1.10e+13 ohm-cm
1.10e+13 ohm-cm
60°C for 500 hrs
Fujipoly Industries Sarcon® 85T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Volume Resistivity 1.10e+13 ohm-cm
1.10e+13 ohm-cm
ASTM D257
Teknor Apex HFFR 2006 Polyolefin, Halogen Free
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing Agency Ratings: IEC Unspecified Rating; ICEA Un..