Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.10e+16 ohm-cm | 1.10e+16 ohm-cm | 150°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30GSR Thin-Film GSR Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm | 1.10e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | 1.10e+16 ohm-cm | 1.10e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Asia Pacific) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | 1.10e+16 ohm-cm | 1.10e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 M-G15 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G0 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G0 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G10 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G10 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G15 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G15 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G15 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G15 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-MFC-G0 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-MFC-G20 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm | 1.10e+16 ohm-cm | C 96/23/96 |
Abatron AboCast 8501-6 One-Component Epoxy AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G0 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G0 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G10 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G10 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT 403 M-G0 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Volume Resistivity | 1.10e+16 ohm-cm @Thickness 2.00 mm |
1.10e+16 ohm-cm @Thickness 0.0787 in |
ASTM D257 |
Beijing Ranger Chem PBT-201-G0 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |