Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.25e+13 ohm-cm | 1.25e+13 ohm-cm | ASTM D257 |
BNZ Materials Transite 1000 Low Temperature Industrial Board These non-asbestos, monolithic fiber cement industrial boards are used in environments up to 1000°F where high strength is the primary concern. These fiber cement boards are used in the foundry ind.. |