Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+10 ohm-cm | 1.30e+10 ohm-cm | |
Pyrotek TS-103 Thermoset Electrical Insulation Product (Nema Grade: G-3) Glass reinforcement, Phenolic resin, Natural color. Good heat resistance. Excellent mechanical and machining properties.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insula.. |