Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+11 ohm-cm | 1.30e+11 ohm-cm | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-n Gap Filler Pad Sarcon GR-n is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Volume Resistivity | 1.30e+11 ohm-cm @Temperature 50.0 °C |
1.30e+11 ohm-cm @Temperature 122 °F |
ASTM D257 |
Teknor Apex APEX® 65014 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |