Polymer Property : Volume Resistivity = 1.30e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+12 ohm-cm
1.30e+12 ohm-cm
ASTM D247
Plenco 00757 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper..
Volume Resistivity 1.30e+12 ohm-cm
1.30e+12 ohm-cm
Tra-Con Tra-Bond 77-1S One Component SMD Adhesive
TRA-BOND 77-1S one component, solvent-free, insulating epoxy adhesive is designed specifically for attaching surface mounted devices (SMDs) to printed circuit boards prior to wave solder. TRA-BOND 7..
Volume Resistivity 1.30e+12 ohm-cm
1.30e+12 ohm-cm
ASTM D247
Plenco 7552 Phenolic, Nodular, Transfer Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..
Volume Resistivity 1.30e+12 ohm-cm
1.30e+12 ohm-cm
Saint-Gobain Korel® K60 Firm Micro-cellular Polyurethane Foam
Description: The Korel® series micro-cellular polyurethane foams are offered in a broad range of properties, making them ideal for a variety of gasketing and energy absorption needs. Korel® microc..