Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.4 ohm-cm | 1.4 ohm-cm | |
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus.. |