Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.46e+13 ohm-cm | 1.46e+13 ohm-cm | |
Dow Corning 3099 HVIC COMPOUND Dow Corning 3099 is a grease-like silicone coating especially formulated to give electrical insulators long-term resistance to water filming and flashover.Features: Protecting electrical insulators... |