Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.58e+12 ohm-cm | 1.58e+12 ohm-cm | ASTM D257 |
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |