Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.59e+10 ohm-cm | 1.59e+10 ohm-cm | ASTM D257 |
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |