Electrical Properties Metric English Comments
Volume Resistivity 1.74e+15 ohm-cm
1.74e+15 ohm-cm
IEC 60093
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic
Novolac resin based, glass fiber and mineral reinforced. Grade with superior stiffness, high dimensional stability and high wear resistance. Good chemical resistance against several fuels at elevate..