Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.90e+14 ohm-cm | 1.90e+14 ohm-cm | 60°C for 500 hrs with 95% RH |
Fujipoly Industries Sarcon® 45Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Volume Resistivity | 1.90e+14 ohm-cm | 1.90e+14 ohm-cm | |
Dow Corning SE 4430 KIT Two-part, thermally conductive elastomer, soft, good thermal conducitvity, UL 94 V-0 rating, low viscosity.Information provided by Dow Corning |
|||
Volume Resistivity | 1.90e+14 ohm-cm | 1.90e+14 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |