Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.10e+12 ohm-cm | 2.10e+12 ohm-cm | 120°C for 1,000 hrs; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-m Gap Filler Pad Sarcon GR-m is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and .. |
|||
Volume Resistivity | 2.10e+12 ohm-cm | 2.10e+12 ohm-cm | ASTM D247 |
Plenco 3554 Phenolic, Granular, Compression Molded PLENCO 03554 is an organic reinforced phenolic molding compound modified with PTFE to offer improved coefficient of friction values. 03554 is available in black. It is UL listed. 03554 is a re-numbe.. |
|||
Volume Resistivity | 2.10e+12 ohm-cm | 2.10e+12 ohm-cm | ASTM D247 |
Plenco 4466 Phenolic, Granular, Compression Molded PLENCO 04466 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength and cosmetic properties. UL recognized under component file E40654. 04466.. |