Electrical Properties Metric English Comments
Volume Resistivity 2.20e+11 ohm-cm
2.20e+11 ohm-cm
ASTM D247
Plenco 2311 Phenolic, Granular, Injection Molded
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr..
Volume Resistivity 2.20e+11 ohm-cm
2.20e+11 ohm-cm
ASTM D247
Plenco 7556 Phenolic, Briquette, Injection Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..