Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.40e+18 ohm-cm | 2.40e+18 ohm-cm | |
Saint-Gobain Rulon® FCJ Grade Bearing/Seal PTFE
(discontinued **) Saint Gobain Rulon® CJ is now produced as a part of the TriStar Plastics Corp. product line under the CJ Bearings trade name.Description: Rulon® is the Saint-Gobain trade name for their family of .. |