Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.41e+18 ohm-cm | 2.41e+18 ohm-cm | |
TriStar CJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |
|||
Volume Resistivity | 2.41e+18 ohm-cm | 2.41e+18 ohm-cm | |
TriStar FCJ Composite Bearing This family of materials offers the combination of high compressive strength, low coefficient of friction, and excellent abrasion and corrosion resistance while running without lubrication. They are.. |