Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.5 ohm-cm | 2.5 ohm-cm | ISO 3915 |
Nanocyl PLASTICYL™ SEBS1001 SEBS (styrene-ethylene/butadiene-styrene) with 10% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Volume Resistivity | 2.5 ohm-cm | 2.5 ohm-cm | ASTM D257 |
Teknor Apex Vidux® CV-1000-91 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-AntistaticForms-PelletsProcessing Method- ExtrusionInformation provided by Teknor Apex Company |
|||
Volume Resistivity | 2.5 ohm-cm | 2.5 ohm-cm | ASTM D257 |
Teknor Apex Vidux® CV-92-A5008A-91 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Antistatic; Conductive; Electromagnetic Shielding (EMI); Non-DEHP Plasticizer; Ethylene Oxide Sterilizable; Radio Frequency Shielding (RFI) Uses: Coating Applications.. |