Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.60e+11 ohm-cm | 2.60e+11 ohm-cm | ASTM D247 |
Plenco 5482 Phenolic, Granular, Injection Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |