Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 210 ohm-cm | 210 ohm-cm | CTM E043 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 3.2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |