Polymer Property : Volume Resistivity = 3.10e+17 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.10e+17 ohm-cm
3.10e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula..
Volume Resistivity 3.10e+17 ohm-cm
3.10e+17 ohm-cm
ASTM D257
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for..
Copyright © lookpolymers.com All Rights Reserved