Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.1e+14 ohm-cm | 3.1e+14 ohm-cm | ASTM D257 |
ALM PA 250 Nylon 12 SLS Prototyping Polymer Highly Recyclable Nylon 12 Laser Sintering Material.Engineered for excellent mechanical properties, part definition and surface finish. Stabilized against thermal degradation resulting in little or.. |