Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.25 ohm-cm @Time 300 sec |
3.25 ohm-cm @Time 0.0833 hour |
25% Carbon Black |
TIMCAL ENSACO™ 260G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |