Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 3.32e+16 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 3.32e+16 ohm-cm
3.32e+16 ohm-cm
ASTM D257
Eastman Cadence™ GS2 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..