Polymer Property : Volume Resistivity = 3.40e+16 ohm-cm
Polymer Property :
Volume Resistivity =
3.40e+16 ohm-cm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
3.40e+16
ohm-cm
>=
3.40e+16
ohm-cm
ASTM D257
SABIC Innovative Plastics Valox® 420SE0U PBT (Asia Pacific)
UV-Stabilized version of 420SE0.