Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.90e+14 ohm-cm | 3.90e+14 ohm-cm | |
Mykroy/Mycalex MM 451 Molding Grade Glass-bonded Mica Composite Natural mica filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets, worldwid.. |
|||
Volume Resistivity | 3.90e+14 ohm-cm | 3.90e+14 ohm-cm | ASTM D257 |
Teknor Apex HFFR 2002 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing Agency Ratings: ICEA Unspecified Rating; IEC Un.. |
|||
Volume Resistivity | 3.90e+14 ohm-cm | 3.90e+14 ohm-cm | E24/125; IPC TM-650 2.5.17.1 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |