Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 30000 ohm-cm | 30000 ohm-cm | 1.5 wt% carbon nanotubes in PC; CTM E043 |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Volume Resistivity | 30000 ohm-cm | 30000 ohm-cm | 1.5 wt% carbon nanotubes in PC; CTM E043 |
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 3 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Volume Resistivity | 30000 ohm-cm | 30000 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |