Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized Information provided by Ravago. |
|||
Volume Resistivity | 4.00e+16 ohm-cm @Temperature 23.0 °C |
4.00e+16 ohm-cm @Temperature 73.4 °F |
100V; ASTM D257 |
Victrex® APTIV® 1300-050G Polyetheretherketone (PEEK) Polymer Film DescriptionAPTIV® 1300 film is the black version of unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance .. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | 500V; Ø 93x3mm; IEC 60093 |
SYNTHOS Forsan® 573 Acrylonitrile Butadiene Styrene (ABS) Increased heat resistant, glossy, good mechanical properties, suitable for electroplating.Applications: Electrotechnics, automotiveHousehold appliances, electric switches, car interior parts, profil.. |
|||
Volume Resistivity | >= 4.00e+16 ohm-cm | >= 4.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 311 PBT Unreinforced, improved resistance to UV. Medium viscosity. |
|||
Volume Resistivity | >= 4.00e+16 ohm-cm | >= 4.00e+16 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics Valox® 312 PBT Unreinforced, For compounding only (not for injection molding), FDA (21 CFR 177.1660) compliant. Medium viscosity.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | >= 4.00e+16 ohm-cm | >= 4.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 315 PBT Unreinforced, For extrusion/compounding only (not for injection molding). High viscosity. Melt viscosity between 7500 and 9500 poise. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 315 PBT (Asia Pacific) General purpose polyester. Fully imported product from USA |
|||
Volume Resistivity | >= 4.00e+16 ohm-cm | >= 4.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics Valox® 830 PBT 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP GF20 CC HF 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High FlowInformation provided by .. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3022A Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3022PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3022PJ is a general use grade.Information provided by Samyang. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3025L1 Polycarbonate, Lens Grade TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3025N1 Polycarbonate, Flame Retardant TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3027IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3027PU(X) Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3027PU(X) is an extrusion grade.Information provided by Samyang. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3030PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3030PJ is a high viscosity gradeInformation provided by Samyang. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3030U Polycarbonate, UV Stabilized TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3500G20 Polycarbonate, 20% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® DMF3000S Polycarbonate, Anti-yellowing PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.DMF3000S is an anti-yellowing grade.Information provided by Samyang. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and.. |
|||
Volume Resistivity | 4.00e+16 - 4.50e+16 ohm-cm | 4.00e+16 - 4.50e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Asia Pacific) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | |
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required.. |
|||
Volume Resistivity | 4.00e+16 - 4.50e+16 ohm-cm | 4.00e+16 - 4.50e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Volume Resistivity | 4.00e+16 - 4.50e+16 ohm-cm | 4.00e+16 - 4.50e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS (Europe-Africa-Middle East) Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® 3025GRU30 Polycarbonate, 30% Glass Reinforced TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electr.. |
|||
Volume Resistivity | 4.00e+16 ohm-cm | 4.00e+16 ohm-cm | ASTM D257 |
Samyang Trirex® TH3022N Polycarbonate, High Flow Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.TH3022N is a high flow, flame retardant grade.Applications: LCD TV, Laptop and Monitor.. |