Polymer Property : Volume Resistivity = 5.80e+12 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 5.80e+12 ohm-cm
5.80e+12 ohm-cm
ASTM D247
Plenco 6343 Phenolic, Granular, Transfer Molded
PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz..