Volume Resistivity 4.0 - 6.0 ohm-cm
4.0 - 6.0 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE002 PC
LNP* STAT-KON* DE002 is a Polycarbonate base resin containing 10% Carbon Fiber. Added feature of this grade is: Electrically Conductive.
Volume Resistivity 4.0 - 6.0 ohm-cm
4.0 - 6.0 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific)
LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber.
Volume Resistivity 4.0 - 6.0 ohm-cm
4.0 - 6.0 ohm-cm
ASTM D257
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.