Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 6.60e+14 ohm-cm
6.60e+14 ohm-cm
DIN IEC 60093
Lushan PJ-1 Polypropylene Compounds for Steel Pipe Top Coats
Polypropylene compound for steel pipe top coats Lushan PJ-1 is used for 3LPP coating system in colored white. It is supplied in pellets for melt extrusion or in a powder for application by spray or ..
Volume Resistivity 6.60e+14 ohm-cm
6.60e+14 ohm-cm
ASTM D257
Teknor Apex HFFR 2004 Polyolefin, Halogen Free
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Uns..
Volume Resistivity 6.60e+14 ohm-cm
6.60e+14 ohm-cm
Dow Corning SILASTIC® 9280/30 KIT PARTS A&B
40 Durometer, 2-part, 1 to 1 mix, translucent Liquid Silicone Rubber.Information provided by Dow Corning