Polymer Property : Volume Resistivity = 6.7e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 6.7e+15 ohm-cm
6.7e+15 ohm-cm
Mykroy/Mycalex MM 601 Molding Grade Glass-bonded Mica Composite
Synthetic/Natural Mica Filler. Does not burn. ROHS Compliant.This ceramoplastic material is a versatile and efficient insulating material designed to meet the exacting demands of technical markets,..
Volume Resistivity 6.7e+15 ohm-cm
6.7e+15 ohm-cm
50% RH; 500V; ASTM D257
ALM PA 620-MF Mineral Fiber Filled Nylon 12 SLS Prototyping Polymer
Information provided by Advanced Laser Materials (ALM).