Polymer Property : Volume Resistivity = 6.90e+10 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 6.90e+10 ohm-cm
6.90e+10 ohm-cm
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M