Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.0 ohm-cm | 7.0 ohm-cm | ASTM D257 |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Volume Resistivity | <= 7.0 ohm-cm | <= 7.0 ohm-cm | without pressure-sensitive adhesive; CEPS-0002 |
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |