Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.00e+13 ohm-cm @Temperature 20.0 °C |
7.00e+13 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 3522D Halogen Free PVC Sheathing; standard grade improved processing speed |
|||
Volume Resistivity | 7.00e+13 ohm-cm | 7.00e+13 ohm-cm | IEC 93 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |