Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 7.50e+9 ohm-cm @Temperature 50.0 °C |
7.50e+9 ohm-cm @Temperature 122 °F |
ASTM D257 |
Teknor Apex APEX® 94-A1235-C-75-NT1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex |
|||
Volume Resistivity | 7.50e+9 ohm-cm | 7.50e+9 ohm-cm | ASTM D257-93 |
Zircar Refractory Composites RSLE-501 CYLINDERS Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-501 is a low expansion high strength reinforced silica matrix composites in a cylindrical form. This material was designed for use as a high strength, durable insul.. |
|||
Volume Resistivity | 7.50e+9 ohm-cm | 7.50e+9 ohm-cm | ASTM D257-93 |
Zircar Refractory Composites RSLE-57 Refractory Sheet ZIRCAR Refractory Sheet Type RSLE-57 is a low expansion high strength reinforced silica matrix composite . This material was designed for use as a high strength insulator in induction hot press appl.. |