Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 8.20e+18 ohm-cm | 8.20e+18 ohm-cm | ASTM D4496 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Volume Resistivity | 8.20e+18 ohm-cm | 8.20e+18 ohm-cm | |
Saint-Gobain Rulon® J Grade Bearing/Seal PTFE Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of f.. |