Polymer Property : Volume Resistivity = 8.40e+11 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 8.40e+11 ohm-cm
8.40e+11 ohm-cm
ASTM D247
Plenco 4414 Phenolic, Granular, Injection Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..