Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.10e+11 ohm-cm | 9.10e+11 ohm-cm | ASTM D247 |
Plenco 3356 Phenolic, Granular, Injection Molded PLENCO 03356 is a mineral filled phenolic molding compound offering excellent arc resistance, comparative tracking, and flame resistant properties. UL recognized under component file E40654. 03356 i.. |