Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.26e+13 ohm-cm | 9.26e+13 ohm-cm | 50% RH; IPC 2.5.17.1 |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |