Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 9.40e+15 ohm-cm | 9.40e+15 ohm-cm | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 30H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |