Polymer Property : Magnetic Saturation Flux Density, Bmax = 11200 Gauss Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Magnetic Saturation Flux Density, Bmax 11200 Gauss
11200 Gauss
Magnetic Induction
Pacific Sintered Materials F-241-S1 Iron Soft Magnetic Powdered Metal
Applications: DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores.Equivalent ASTM Specification: B310-70, TYPE III, CLASS AAll information provided by P..