Electrical Properties | Metric | English | Comments |
---|---|---|---|
Magnetic Saturation Flux Density, Bmax | 13 Gauss | 13 Gauss | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1601 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Magnetic Saturation Flux Density, Bmax | 13 Gauss | 13 Gauss | |
PSM Industries Pacific Sintered Metals Silicon Iron FS-1602 Powdered Metal DC magnetic applications such as armatures, relays, solenoids, pole pieces and cores. Possible AC usesInformation Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Magnetic Saturation Flux Density, Bmax | 13 Gauss | 13 Gauss | |
PSM Industries Pacific Sintered Metals Iron F-241-T Powdered Metal DC magnetic applications such as pole pieces, cores, armatures, generator rotors and stator cores Equivalent ASTM Spec: B310-70, Type V, Class AInformation Provided by Pacific Sintered Metals, a di.. |