Polymer Property : Volume Resistivity = 1.00e+7 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 250 °C
1.00e+7 ohm-cm

@Temperature 482 °F
DIN 52326
Schott Nextrema® 712-3 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 250 °C
1.00e+7 ohm-cm

@Temperature 482 °F
DIN 52326
Schott Nextrema® 724-5 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 250 °C
1.00e+7 ohm-cm

@Temperature 482 °F
DIN 52326
Schott Nextrema® 724-8 Glass Ceramic
The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal..
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 500 °C
1.00e+7 ohm-cm

@Temperature 932 °F
CeramTec Frequenta® Steatite
Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be..
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 600 °C
1.00e+7 ohm-cm

@Temperature 1110 °F
ASTM-D1829
CeramTec Rubalit® 600 Alumina, 48%
Rubalit® 600 is suitable for both mechanical and laser trimming and is chiefly used as the core for high-grade carbon-film resistors.
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 800 °C
>= 1.00e+7 ohm-cm

@Temperature 1470 °F
CeramTec Rubalit® A 1894 Alumina, 94%
Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 800 °C
>= 1.00e+7 ohm-cm

@Temperature 1470 °F
IEC 672-1
CeramTec Rubalit® A 1999.5 Alumina, 99.7%
Rubalit® A 1999.5 (99.7%) is mechanically stronger, features a higher heat conductivity, and is more corrosion resistant than other aluminas. This high-purity aluminum oxide ceramic with carbon mat..
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 400 °C
1.00e+7 ohm-cm

@Temperature 752 °F
IEC 345
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua..
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 800 °C
>= 1.00e+7 ohm-cm

@Temperature 1470 °F
IEC 672-1
CeramTec Rubalit® IS 95 Alumina
Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva..
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 700 °C
>= 1.00e+7 ohm-cm

@Temperature 1290 °F
ASTM-D1829
CoorsTek ADS-995R MidFilm™ 99.5% Alumina Thick Film
Applications: thick films and lasers
Volume Resistivity 1.00e+7 ohm-cm

@Temperature 175 °C
1.00e+7 ohm-cm

@Temperature 347 °F
ASTM D257
3M Scotchcast™ 265 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 265 is a new solution to an old problem. Historically, manufactures of coils, stators and armatures have used liquid-based varnishes or resins to coat and impregnate t..
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 800 °C
>= 1.00e+7 ohm-cm

@Temperature 1470 °F
IEC 672-1
CeramTec Rubalit® A 1896 Alumina
Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele..
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 800 °C
>= 1.00e+7 ohm-cm

@Temperature 1470 °F
CeramTec Rubalit® A 1898 Alumina, 98%
Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..