Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.30e+9 ohm-cm @Temperature 250 °C |
1.30e+9 ohm-cm @Temperature 482 °F |
|
Schott Glass 8689 Borosilicate Glass Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium.. |
|||
Volume Resistivity | 1.30e+9 ohm-cm @Temperature 25.0 °C |
1.30e+9 ohm-cm @Temperature 77.0 °F |
cured 30 days @ 25°C |
Abatron AboCast 8110-1/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |