Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.50e+16 ohm-cm @Temperature 75.0 °C |
1.50e+16 ohm-cm @Temperature 167 °F |
|
Master Bond EP112 Low Viscosity Heat Curing Cycloaliphatic Epoxy Adhesive Master Bond Polymer System EP112 is a solventless, low viscosity two component cycloaliphatic epoxy resin system which is specifically designed for high performance outdoor and indoor electrical & e.. |