Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 10 ohm-cm @Temperature 400 °C |
10 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec CD 110 Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. It outstanding sliding properties and high thermal conductivity make useful in tribological applicati.. |
|||
Volume Resistivity | <= 10 ohm-cm @Temperature 400 °C |
<= 10 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rocar® S Silicon Carbide, SSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |
|||
Volume Resistivity | 10 ohm-cm @Temperature 400 °C |
10 ohm-cm @Temperature 752 °F |
IEC 672-1 |
CeramTec Rocar® ST Silicon Carbide, SSiC Silicon carbide is extremely hard and displays excellent corrosion and thermal shock resistance. Its outstanding sliding properties and high thermal conductivity make useful in tribological applicat.. |