Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.10e+15 ohm-cm @Temperature 50.0 °C |
2.10e+15 ohm-cm @Temperature 122 °F |
ASTM D257 |
Teknor Apex Telcar® TL-1522G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Volume Resistivity | 2.10e+15 ohm-cm @Temperature 25.0 °C |
2.10e+15 ohm-cm @Temperature 77.0 °F |
|
Atom Adhesives AA-SUPERTHERM 05 Epoxy Adhesive AA-SUPERTHERM 05 is a thixotropic (smooth paste) Pure Diamond ultra-high thermally conductive epoxy two-part adhesive that develops strong, durable, high-impact bonds at room temperature which impro.. |