Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 5.00e+14 ohm-cm @Temperature 20.0 °C |
5.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec RK 87 Alumina, 99.8% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Volume Resistivity | 5.00e+14 ohm-cm @Temperature 30.0 °C |
5.00e+14 ohm-cm @Temperature 86.0 °F |
JIS-K-6723 |
Denka VINYKON W4050 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 5.00e+14 ohm-cm @Temperature 30.0 °C |
5.00e+14 ohm-cm @Temperature 86.0 °F |
JIS-K-6723 |
Denka VINYKON W4200 PVC, W grade for equipment cords, for heat resistance A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 5.00e+14 ohm-cm @Temperature 30.0 °C |
5.00e+14 ohm-cm @Temperature 86.0 °F |
JIS-K-6723 |
Denka VINYKON W5230 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Volume Resistivity | 5.00e+14 ohm-cm @Temperature 20.0 °C |
5.00e+14 ohm-cm @Temperature 68.0 °F |
IEC 672-1 |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |