Electrical Properties Metric English Comments
Volume Resistivity 5.00e+8 ohm-cm

@Temperature 400 °C
5.00e+8 ohm-cm

@Temperature 752 °F
IEC 672-1
CeramTec RK 87 Alumina, 99.8%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.
Volume Resistivity 5.00e+8 ohm-cm

@Temperature 400 °C
5.00e+8 ohm-cm

@Temperature 752 °F
IEC 672-1
CeramTec AT 79 Alumina, 99.6%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.